Book Role of Hydrogen in Hot salt Stress corrosion of a Titanium Alloy

Download or read book Role of Hydrogen in Hot salt Stress corrosion of a Titanium Alloy written by Hugh R. Gray and published by . This book was released on 1971 with total page 36 pages. Available in PDF, EPUB and Kindle. Book excerpt: Hydrogen embrittlement during hot salt, stress corrosion of titanium alloys.

Book NASA Technical Note

    Book Details:
  • Author :
  • Publisher :
  • Release : 1972
  • ISBN :
  • Pages : 602 pages

Download or read book NASA Technical Note written by and published by . This book was released on 1972 with total page 602 pages. Available in PDF, EPUB and Kindle. Book excerpt:

Book Corrosion of Titanium

Download or read book Corrosion of Titanium written by J. D. Jackson and published by . This book was released on 1966 with total page 54 pages. Available in PDF, EPUB and Kindle. Book excerpt:

Book NASA Technical Memorandum

Download or read book NASA Technical Memorandum written by and published by . This book was released on 1974 with total page 158 pages. Available in PDF, EPUB and Kindle. Book excerpt:

Book An Electrochemical Model for Hot salt Stress corrosion of Titanium Alloys

Download or read book An Electrochemical Model for Hot salt Stress corrosion of Titanium Alloys written by Marvin Garfinkle and published by . This book was released on 1972 with total page 44 pages. Available in PDF, EPUB and Kindle. Book excerpt: An electrochemical model of hot-salt stress-corrosion cracking of titanium alloys is proposed based on an oxygen-concentration cell. Hydrogen embrittlement is proposed as the direct cause of cracking, the hydrogen being generated as the results of the hydrolysis of complex halides formed at the shielded anode of the electrochemical cell. The model found to be consistent with the diverse observations made both in this study and by many investigators in this field.

Book Scientific and Technical Aerospace Reports

Download or read book Scientific and Technical Aerospace Reports written by and published by . This book was released on 1981 with total page 788 pages. Available in PDF, EPUB and Kindle. Book excerpt:

Book Aerospace Structural Materials

Download or read book Aerospace Structural Materials written by and published by . This book was released on 1970 with total page 344 pages. Available in PDF, EPUB and Kindle. Book excerpt:

Book The Science  Technology and Application of Titanium

Download or read book The Science Technology and Application of Titanium written by R. I. Jaffee and published by Elsevier. This book was released on 2013-09-24 with total page 1225 pages. Available in PDF, EPUB and Kindle. Book excerpt: The Science, Technology and Application of Titanium contains the proceedings of an International Conference organized by the Institute of Metals, The Metallurgical Society of AIME, and the American Society for Metals in association with the Japan Institute of Metals and the Academy of Sciences of the USSR and held at the Royal Festival Hall in London, on May 21-24, 1968. The papers explore scientific and technological developments as well as applications of titanium and cover topics ranging from processing of titanium to its chemical and environmental behavior, physics, thermodynamics, and kinetics. Deformation and fracture, phase transformations and heat treatment, and alloying are also discussed. This book is comprised of 114 chapters and begins with an overview of the titanium industry in Europe and the United States. The reader is then introduced to primary and secondary fabrication of titanium; corrosion and oxidation; physical properties of titanium alloys; interaction of titanium with elements of the periodic system; and elastic interactions between dislocations and twin and grain boundaries in titanium. The crystallography of deformation twinning in titanium is also examined, along with superplasticity and transformation plasticity in titanium. The remaining chapters focus on interstitial strengthening of titanium alloys; mechanism of martensitic transformation in titanium and its alloys; phase relationships in titanium-oxygen alloys; strengthening of titanium alloys by shock deformation; and titanium hot forming. This monograph will be of interest to chemists and metallurgists.

Book Handbook of Corrosion Data

Download or read book Handbook of Corrosion Data written by Bruce D. Craig and published by ASM International. This book was released on 1994-12-31 with total page 1026 pages. Available in PDF, EPUB and Kindle. Book excerpt: This book makes it easy for you to find what effect environment has on the corrosion of metals and alloys. However, this volume offers information on additional environments including concrete, soil, groundwater, distilled water, sodium acetate and more. ThereAs also updated and expanded coverage of previously discussed environments as well as information on environments which deal with the dairy, food, brewing, aerospace, petrochemical and building industries. The environments are listed alphabetically. Each listing includes a general description of the conditions, a comment on the corrosion characteristics of various alloys in such a situation, a bibliography of recent articles specific to the environment, tables consolidating and comparing corrosion rates at various temperatures and concentrations for various alloys, and graphical information. Also included are summaries on the general corrosion characteristics of major metals and alloys.

Book Nuclear Science Abstracts

Download or read book Nuclear Science Abstracts written by and published by . This book was released on 1969 with total page 1254 pages. Available in PDF, EPUB and Kindle. Book excerpt:

Book Applications Related Phenomena in Titanium Alloys

Download or read book Applications Related Phenomena in Titanium Alloys written by Conrad H. and published by ASTM International. This book was released on 1968 with total page 300 pages. Available in PDF, EPUB and Kindle. Book excerpt:

Book Stress corrosion Cracking of Titanium

Download or read book Stress corrosion Cracking of Titanium written by and published by . This book was released on 1966 with total page 280 pages. Available in PDF, EPUB and Kindle. Book excerpt:

Book NASA Scientific and Technical Reports

Download or read book NASA Scientific and Technical Reports written by United States. National Aeronautics and Space Administration Scientific and Technical Information Division and published by . This book was released on 1968 with total page 478 pages. Available in PDF, EPUB and Kindle. Book excerpt:

Book A Selected Listing of NASA Scientific and Technical Reports

Download or read book A Selected Listing of NASA Scientific and Technical Reports written by United States. National Aeronautics and Space Administration. Scientific and Technical Information Division and published by . This book was released on 1969 with total page 470 pages. Available in PDF, EPUB and Kindle. Book excerpt: