Download or read book Stress Corrosion Cracking of Austenitic Stainless Steel written by McIntyre R. Louthan and published by . This book was released on 1964 with total page 24 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book The Susceptibility of Austenitic Stainless Steels to Stress Corrosion Cracking written by W. O. Binder and published by . This book was released on 1945 with total page 10 pages. Available in PDF, EPUB and Kindle. Book excerpt: Occasionally in the application of the austenitic chromium-nickel steels to corrosive conditions, failures have occurred by cracking without serious general over-all attack of the metal. As pointed out by Hoyt and Scheil(1), and by Scheil, et al.(2) as well as by Hodge and Miller(3), the stress-corrosion failures that have occurred have been limited in number, and have taken place only when the steels were exposed to certain corrodents. These investigators have stated that while stress-corrosion cracking can be intergranular in nature and originate at the grain boundaries of the austenitic chromium-nickel steels, it can also take place in transgranular fashion. They have shown that the cracking may be either initiated at the grain boundaries and may propagate along grain boundaries for some distance and then suddenly extend across grains, or it may begin in a transgranular fashion and suddenly proceed along grain boundaries until the cracking stops. Their data further show that when austenitic stainless steel is subject to intergranular attack, stress will concentrate and cause cracking in service.
Download or read book The Susceptibility of Six Stainless Steels to Stress Corrosion at Ambient and Elevated Temperatures written by David N. Braski and published by . This book was released on 1964 with total page 32 pages. Available in PDF, EPUB and Kindle. Book excerpt: The susceptibility of six stainless steels to stress corrosion has been determined by exposing self-stressed specimens indoors and outdoors at ambient temperatures and also at 550 F (56l K). The salt-coated stainless steels were resistant to stress corrosion cracking at 550 F (56l K) for exposures from 4000 to 10,000 hours. Specimens of AM-350 DA and AM-367 stainless steel were found to be very susceptible to stress-corrosion cracking with exposures less than 5000 hours in both the indoor (with a salt coating) and outdoor (with and without a salt coating) environments, while the AM-350 CRT, AISI 501, PH l5-7 Mo, and PH 14-8 Mo displayed excellent resistance. In general, the stainless steels with higher austenite contents appeared to have better resistance to the corrosive effects of salt, both at rooni temperature and at 550 F (56l K).
Download or read book Evaluation of Stress Corrosion Cracking Susceptibility of Austenitic Stainless Steels in CaCl2 Solution by the Constant Load Method written by Heikki Leinonen and published by . This book was released on 1995 with total page 53 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book The Mechanism of Stress Corrosion Cracking of Austenitic Stainless Steels written by Julius J. Harwood and published by . This book was released on 1960 with total page 8 pages. Available in PDF, EPUB and Kindle. Book excerpt: The purpose of this discussion is to assess the state of our understanding concerning the factors and mechanism(s) which determine and control the susceptibility to stress-corrosion cracking of the austenitic stainless steels. The growing importance of this problem has led to a considerable amount of research, both in this country and abroad, aimed at delineating more specifically the environmental, compositional, and structural conditions involved and at elucidating the underlying mechanism for the cracking phenomenon. As a result of this research effort, a number of mechanisms have been proposed, but all appear to contain certain deficiencies in explaining certain of the characteristic features of the stress-corrosion cracking process; that is to say, unequivocal arguments cannot be presented in behalf of any of the proposed mechanisms. Possibly more to the point is the fact that few of the currently debated mechanisms have yielded critical clues which could lead to compositional or structural modifications of commercial materials to reduce or prevent the incidence of cracking. It is encouraging to note, however, that the more recent experimental evidence is developing a basis whereby critical type of experiments can be designed to differentiate clearly the mode of damage.
Download or read book Stress Corrosion New Approaches written by H. L. Craig and published by ASTM International. This book was released on 1976 with total page 444 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Corrosion of Austenitic Stainless Steels written by H S Khatak and published by Woodhead Publishing. This book was released on 2002-10-14 with total page 436 pages. Available in PDF, EPUB and Kindle. Book excerpt: This comprehensive study covers all types of corrosion of austenitic stainless steel. It also covers methods for detecting corrosion and investigating corrosion-related failure, together with guidelines for improving corrosion protection of steels. Details all types of corrosion of austenitic stainless steel Covers methods for detecting corrosion and investigating corrosion-related failure Outlines guidelines for improving corrosion protection of steels
Download or read book Stress Corrosion Cracking written by V S Raja and published by Elsevier. This book was released on 2011-09-22 with total page 817 pages. Available in PDF, EPUB and Kindle. Book excerpt: The problem of stress corrosion cracking (SCC), which causes sudden failure of metals and other materials subjected to stress in corrosive environment(s), has a significant impact on a number of sectors including the oil and gas industries and nuclear power production. Stress corrosion cracking reviews the fundamentals of the phenomenon as well as examining stress corrosion behaviour in specific materials and particular industries.The book is divided into four parts. Part one covers the mechanisms of SCC and hydrogen embrittlement, while the focus of part two is on methods of testing for SCC in metals. Chapters in part three each review the phenomenon with reference to a specific material, with a variety of metals, alloys and composites discussed, including steels, titanium alloys and polymer composites. In part four, the effect of SCC in various industries is examined, with chapters covering subjects such as aerospace engineering, nuclear reactors, utilities and pipelines.With its distinguished editors and international team of contributors, Stress corrosion cracking is an essential reference for engineers and designers working with metals, alloys and polymers, and will be an invaluable tool for any industries in which metallic components are exposed to tension, corrosive environments at ambient and high temperatures. - Examines the mechanisms of stress corrosion cracking (SCC) presenting recognising testing methods and materials resistant to SCC - Assesses the effect of SCC on particular metals featuring steel, stainless steel, nickel-based alloys, magnesium alloys, copper-based alloys and welds in steels - Reviews the monitoring and management of SCC and the affect of SCC in different industries such as petrochemical and aerospace
Download or read book Stress corrosion Cracking of Stainless Steel written by Myra S. Feldman and published by . This book was released on 1962 with total page 72 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress corrosion Cracking of High strength Stainless Steels in Atmospheric Environments written by C. J. Slunder and published by . This book was released on 1961 with total page 44 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress Corrosion Cracking Susceptibility Index ISCC of Austenitic Stainless Steels in Constant Strain Rate Test written by S. Abe and published by . This book was released on 1979 with total page 11 pages. Available in PDF, EPUB and Kindle. Book excerpt: A new stress corrosion cracking (SCC) susceptibility index, ISCC, is proposed in constant strain rate SCC test both for transgranular (TG)SCC and for inter-granular (IG)SCC. ISCC is best defined by the equation Isec=Asec/Amech are the area of SCC fractured surface and that of mechanically fractured surface, respectively. It is found that there is a good correlation between ISCC in constant strain-rate test and the time to fracture in constant load test.
Download or read book Stress corrosion Cracking written by Warren E. Berry and published by . This book was released on 1961 with total page 36 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress corrosion cracking susceptibility of bonding zone of austenitic stainless steel overlaying INTERNATIONAL INSTITUTE OF WELDING IX 1778 written by T. Hara and published by . This book was released on 1994 with total page 0 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress corrosion Cracking written by Russell H. Jones and published by ASM International(OH). This book was released on 1992 with total page 466 pages. Available in PDF, EPUB and Kindle. Book excerpt: Details the many conditions under which stress-corrosion cracking (SCC) can occur, the parameters which control SCC, and the methodologies for mitigating and testing for SCC, plus information on mechanisms of SCC with experimental data on a variety of materials. Contains information about environmen
Download or read book Report on Stress corrosion Cracking of Austenitic Chromium nickel Stainless Steels written by American Society for Testing Materials. Committee A-10 on Iron-Chromium, Iron-Chromium-Nickel, and Related Alloys and published by . This book was released on 1960 with total page 108 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Transgranular Stress Corrosion Cracking in Austenitic Stainless Steels written by Dwaine Leroy Klarstrom and published by . This book was released on 1966 with total page 128 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Relative Humidity and the Susceptibility of Austenitic Stainless Steel to Stress Corrosion Cracking in an Impure Plutonium Oxide Environment written by and published by . This book was released on 2010 with total page pages. Available in PDF, EPUB and Kindle. Book excerpt: Laboratory tests to investigate the corrosivity of moist plutonium oxide/chloride salt mixtures on 304L and 316L stainless steel coupons showed that corrosion occurred in selected samples. The tests exposed flat coupons for pitting evaluation and 'teardrop' stressed coupons for stress corrosion cracking (SCC) evaluation at room temperature to various mixtures of PuO2 and chloride-bearing salts for periods up to 500 days. The exposures were conducted in sealed containers in which the oxide-salt mixtures were loaded with about 0.6 wt % water from a humidified helium atmosphere. Observations of corrosion ranged from superficial staining to pitting and SCC. The extent of corrosion depended on the total salt concentration, the composition of the salt and the moisture present in the test environment. The most significant corrosion was found in coupons that were exposed to 98 wt % PuO2, 2 wt % chloride salt mixtures that contained calcium chloride and 0.6 wt% water. SCC was observed in two 304L stainless steel teardrop coupons exposed in solid contact to a mixture of 98 wt % PuO2, 0.9 wt % NaCl, 0.9 wt % KCl, and 0.2 wt % CaCl2. The cracking was associated with the heat-affected zone of an autogenous weld that ran across the center of the coupon. Cracking was not observed in coupons exposed to the headspace gas above the solid mixture, or in coupons exposed to other mixtures with either no CaCl2 or 0.92 wt% CaCl2. SCC was present where the 0.6 wt % water content exceeded the value needed to fully hydrate the available CaCl2, but was absent where the water content was insufficient. These results reveal the significance of the relative humidity in the austenitic stainless steels environment to their susceptibility to corrosion. The relative humidity in the test environment was controlled by the water loading and the concentration of the hydrating salts such as CaCl2. For each salt or salt mixture there is a threshold relative humidity below which the necessary liquid electrolyte cannot exist, and therefore below which the SCC risk is very low. This threshold is a thermodynamic quantity known as the deliquescence relative humidity that is dependent on the identity of the salt but is independent of the quantity of salt. Below the deliquescence RH there should be low corrosion risk, and above it the corrosion risk increases rapidly as a liquid phase, which is initially saturated with salt, grows and becomes more widespread in the container.