Download or read book Stress corrosion Cracking Tests on Some High strength Steels Using Theusnrl Cantilever Method written by Canada. Mines Branch and published by . This book was released on 1969 with total page pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress corrosion on Cracking Tests on Some High strength Steels Using the UNSRL Cantilever Method written by Canada. Mines Branch and published by . This book was released on 1969 with total page pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress corrosion Cracking in High Strength Steels and in Titanium and Aluminum Alloys written by Benjamin Floyd Brown and published by . This book was released on 1972 with total page 390 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress corrosion Cracking of High strength Stainless Steels in Atmospheric Environments written by C. J. Slunder and published by . This book was released on 1961 with total page 44 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress Corrosion Cracking Of Metals A State of the Art written by H. Lee Craig and published by ASTM International. This book was released on 1972 with total page 174 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress corrosion Cracking and Related Phenomena in High strength Steels a Review of the Problem with an Annotated Bibliography written by B. F. Brown and published by . This book was released on 1963 with total page 25 pages. Available in PDF, EPUB and Kindle. Book excerpt: The problem of the stress-corrosion cracking of high-strength steels in contrasted with stress corrosion in other metals. The implications of hydrogen embrittlement and especially of brittle fracture to interpretations of stress-corrosion cracking tests on high-strength steels are summarized. Test methods are briefly described, and the results of recent studies as reported in the literature are summarized topically. A discussion of the meaning of these findings is given, together with recommendations regarding the further development of test concepts. An annotated bibliography of thirty-six entries is appended. (Author).
Download or read book Exploratory Stress corrosion Cracking Tests on Some Low alloy High strength Steels written by G. J. Biefer and published by . This book was released on 1969 with total page 15 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Influence of Experimental Variables on the Measurement of Stress Corrosion Cracking Properties of High Strength Steels written by TW. Crooker and published by . This book was released on 1990 with total page 13 pages. Available in PDF, EPUB and Kindle. Book excerpt: A systematic investigation was undertaken to examine the influence of experimental variables on the measurement of stress corrosion cracking (SCC) properties of two high-strength steels using fracture mechanics test procedures. The properties of interest were the SCC threshold stress-intensity (KISCC) and time-based crack growth rate (da/dt). Two quench-and-tempered alloy steels in the form of rolled plate material were tested. The steel had yield strengths of 965 MPa (140 ksi) and 1207 MPa (175 ksi). The primary experimental variables investigated included: (1) specimen type (bolt-loaded wedge-opening loaded (WOL) and cantilever beam); (2) bulk solution chemistry (3.5% NaCl in distilled water and natural seawater); (3) dissolved oxygen content of the bulk solution; (4) electrode potential (open circuit and -1.0 V versus Ag/AgCl); (5) method of applying cathodic protection (potentiostat and zinc couple; (6) precracking stress-intensity level; (7) initial applied stress-intensity level; and (8) test duration. The effects of these experimental variables on KISCC and da/dt measurement are reported and the implications of these findings on test method development are discussed.
Download or read book Stress corrosion Cracking written by Russell H. Jones and published by ASM International(OH). This book was released on 1992 with total page 466 pages. Available in PDF, EPUB and Kindle. Book excerpt: Details the many conditions under which stress-corrosion cracking (SCC) can occur, the parameters which control SCC, and the methodologies for mitigating and testing for SCC, plus information on mechanisms of SCC with experimental data on a variety of materials. Contains information about environmen
Download or read book Stress Corrosion Cracking in High Strength Steels and in Titanium and Aluminum Alloys written by Brown BF Ed and published by . This book was released on 1972 with total page pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Investigation of Stress corrosion Cracking of High Strength Steels written by and published by . This book was released on 1964 with total page 15 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress Corrosion Cracking in High Strength Steels written by Ming Tsung Wang and published by . This book was released on 1972 with total page 612 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress Corrosion Cracking of High Strength Steels with Particular Reference to Welding written by T. G. Gooch and published by . This book was released on 1975 with total page pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress corrosion Cracking of High Strength Steels and Titanium Alloys written by and published by . This book was released on 1972 with total page 30 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress corrosion Cracking in High Strength Steels and in Tatanium and Aluminum Alloys written by United States. Naval Research Office and published by . This book was released on 1972 with total page 366 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Mechanism of stress corrosion cracking in welded high strength steels written by T. G. Gooch and published by . This book was released on 1969 with total page 0 pages. Available in PDF, EPUB and Kindle. Book excerpt: