Download or read book Stress Corrosion Cracking Resistance of Alloys 600 and 690 and Compatible Weld Metals in BWRs written by and published by . This book was released on 1988 with total page pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress Corrosion Cracking Resistance of Alloys 600 and 690 and Compatible Weld Metals in BWRs written by Electric Power Research Institute and published by . This book was released on 1988 with total page pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress corrosion cracking of Alloys 600 and 690 and weld metals No 82 and No 182 in high temperature water interim report written by R. A. Page and published by . This book was released on 1982 with total page 0 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress Corrosion Cracking of Alloys 600 and 690 and Weld Metals No 82 and No 182 in High temperature Water written by and published by . This book was released on 1982 with total page pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Energy Research Abstracts written by and published by . This book was released on 1988 with total page 500 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Ninth International Symposium on Environmental Degradation of Materials in Nuclear Power Systems written by Steve Bruemmer and published by John Wiley & Sons. This book was released on 2013-10-18 with total page 1776 pages. Available in PDF, EPUB and Kindle. Book excerpt: This collection presents an exchange of ideas among scientists and engineers about the economic and safety concerns surrounding environmentally induced materials problems which lead to nuclear power plant outages. Scientists and engineers concerned with the environmental degradation processes (corrosion, mechanical, and radiation effects) present their latest results on such topics as life extension/relicensing and materials problems associated with spent fuel storage and radioactive waste disposal. This collection will be of interest to utility engineers, reactor vendor engineers, plant architect engineers, researchers concerned with materials degradation, and consultants involved in design, construction, and operation of water reactors.
Download or read book Indications of Stress Corrosion Cracking Resistance in Alloy 82 Dissimilar Metal Welds in Simulated Primary Water Environments written by Suraj Persaud and published by . This book was released on 2011 with total page 220 pages. Available in PDF, EPUB and Kindle. Book excerpt: Joints between carbon steel and Alloy 600, containing Alloy 82 weld metal, were exposed to two steam-hydrogen environments considered to simulate exposure to primary water conditions in a Pressurized Water Reactor (PWR) or Canada Deuterium Uranium (CANDU) reactor. The welds were found to have elevated and variable iron contents due to dilution by carbon steel during welding. This gave the Alloy 82 weld, near the inner surface of the component, an iron content approaching that of Alloy 800. A potentially protective external iron oxide film formed on the inner surface of the weld. However, the chromium content throughout the weld is below that which would form an external chromium oxide. The results indicate that low chromium content causes internal oxidation throughout the weld and potentially below the external iron oxide which could lead to Primary Water Stress Corrosion Cracking (PWSCC).
Download or read book Stress Corrosion Cracking written by V S Raja and published by Elsevier. This book was released on 2011-09-22 with total page 817 pages. Available in PDF, EPUB and Kindle. Book excerpt: The problem of stress corrosion cracking (SCC), which causes sudden failure of metals and other materials subjected to stress in corrosive environment(s), has a significant impact on a number of sectors including the oil and gas industries and nuclear power production. Stress corrosion cracking reviews the fundamentals of the phenomenon as well as examining stress corrosion behaviour in specific materials and particular industries.The book is divided into four parts. Part one covers the mechanisms of SCC and hydrogen embrittlement, while the focus of part two is on methods of testing for SCC in metals. Chapters in part three each review the phenomenon with reference to a specific material, with a variety of metals, alloys and composites discussed, including steels, titanium alloys and polymer composites. In part four, the effect of SCC in various industries is examined, with chapters covering subjects such as aerospace engineering, nuclear reactors, utilities and pipelines.With its distinguished editors and international team of contributors, Stress corrosion cracking is an essential reference for engineers and designers working with metals, alloys and polymers, and will be an invaluable tool for any industries in which metallic components are exposed to tension, corrosive environments at ambient and high temperatures. - Examines the mechanisms of stress corrosion cracking (SCC) presenting recognising testing methods and materials resistant to SCC - Assesses the effect of SCC on particular metals featuring steel, stainless steel, nickel-based alloys, magnesium alloys, copper-based alloys and welds in steels - Reviews the monitoring and management of SCC and the affect of SCC in different industries such as petrochemical and aerospace
Download or read book Proceedings of the Eighth International Symposium on Environmental Degradation of Materials in Nuclear Power Systems Water Reactors written by and published by . This book was released on 1997 with total page 496 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Corrosion written by and published by . This book was released on 1991-07 with total page 532 pages. Available in PDF, EPUB and Kindle. Book excerpt: Issues include special section called Corrosion abstracts.
Download or read book Corrosion Resistance of Steels Nickel Alloys and Zinc in Aqueous Media written by Michael Schütze and published by John Wiley & Sons. This book was released on 2016-01-05 with total page 418 pages. Available in PDF, EPUB and Kindle. Book excerpt: This handbook is derived from the online reference "Corrosion Handbook", bringing together the relevant information about corrosion protection and prevention for steels, one of the most widely used materials. It provides comprehensive information, including tabulated data and references, on the corrosion properties of the following materials: Unalloyed steels and cast steel, unalloyed cast iron, high-alloy cast iron, high-silicon cast iron, structural steels with up to 12% chromium, ferritic chromium steels with more than 12% chromium, ferritic-austenitic steels with more than 12% chromium, high-alloy multiphase steels, ferritic/perlitic-martensitic steels, ferritic-austenitic steels/duplex steels, austenitic chromium-nickel steels, austenitic chromium-nickel-molybdenum steels, austenitic chromium-nickel steels with special alloying additions, special iron-based alloys, and zinc. The following corrosive media are considered: Seawater, brackish water, industrial waste water, municipal waste water, drinking water, high-purity water.
Download or read book Primary Water Stress Corrosion Cracking of Alloy 600 written by and published by . This book was released on 1993 with total page 13 pages. Available in PDF, EPUB and Kindle. Book excerpt: Correlations of stress corrosion cracking (SCC) data in deaerated water with temperature, stress, metallography, and processing for laboratory test specimens are presented. Initiation time data show that a low temperature anneal and resulting absence of grain boundary carbides result in a material having increased susceptibility to SCC. Data also show that hot worked and annealed Alloy 600 is more resistant than cold worked and annealed material, both having carbide decorated grain boundaries. In absence of grain boundary carbides, both materials are equally susceptible. Low temperature thermal treatment (1100F) reduces SCC susceptibility with or without grain boundary decoration. Weld metal data and data correlations developed from 700 double U-bends are presented. Data demonstrate the effect of increased carbon content to improve SCC resistance. The data shows that the general relation of time, temperature and strain for wrought material is followed for the weld metal. The weld process used did not affect the SCC susceptibility of EN-82 which showed a greater resistance to SCC than EN-62. Stress relief of weld deposits showed an improvement for wrought material. Heat affected zone resistance was improved if the starting material received a high temperature anneal (1850 to 2000F). Range of SCC initiation times for weld metal is comparable to the range of initiation times for wrought material.
Download or read book Stress corrosion Cracking in High Strength Steels and in Titanium and Aluminum Alloys written by Benjamin Floyd Brown and published by . This book was released on 1972 with total page 388 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Stress corrosion Cracking written by Russell H. Jones and published by ASM International(OH). This book was released on 1992 with total page 466 pages. Available in PDF, EPUB and Kindle. Book excerpt: Details the many conditions under which stress-corrosion cracking (SCC) can occur, the parameters which control SCC, and the methodologies for mitigating and testing for SCC, plus information on mechanisms of SCC with experimental data on a variety of materials. Contains information about environmen
Download or read book Metals Abstracts written by and published by . This book was released on 1998 with total page 1076 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Materials Transactions written by and published by . This book was released on 2007 with total page 668 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Proceedings of the Third International Symposium on Environmental Degradation of Materials in Nuclear Power Systems Water Reactors written by George J. Theus and published by . This book was released on 1987 with total page 870 pages. Available in PDF, EPUB and Kindle. Book excerpt: