Download or read book Grain by Grain Study of the Mechanisms of Crack Propagation During Iodine Stress Corrosion Cracking of Zircaloy 4 written by AO. Dorado and published by . This book was released on 1994 with total page 17 pages. Available in PDF, EPUB and Kindle. Book excerpt: This paper describes the tests conducted to determine the conditions leading to cracking of a specified grain of metal, during the iodine stress corrosion cracking (SCC) of zirconium alloys, focusing on the crystallographic orientation of crack paths, the critical stress conditions, and the significance of the fractographic features encountered. In order to perform crystalline orientation of fracture surfaces, a specially heat-treated Zircaloy-4 having very large grains, grown up to the wall thickness, was used. Careful orientation work has proved that intracrystalline pseudo-cleavage occurs only along basal planes. The effects of anisotropy, plasticity, triaxiality, and residual stresses originated in thermal contraction have to be considered to account for the influence of the stress state. A grain-by-grain calculation led to the conclusion that transgranular cracking always takes place on those bearing the maximum resolved tensile stress perpendicular to basal planes. Propagation along twin boundaries has been identified among the different fracture modes encountered.
Download or read book Proceedings of the 15th International Conference on Environmental Degradation of Materials in Nuclear Power Systems Water Reactors written by Gabriell Ilevbare and published by Springer. This book was released on 2017-07-17 with total page 2354 pages. Available in PDF, EPUB and Kindle. Book excerpt: This 15th Edition of the International Conference on Materials Degradation in Light Water Reactors focuses on subject areas critical to the safe and efficient running of nuclear reactor systems through the exchange and discussion of reseach results as well as field operating and management experience.
Download or read book Zirconium in the Nuclear Industry Tenth International Symposium written by A. M. Garde and published by ASTM International. This book was released on 1994 with total page 805 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Energy Research Abstracts written by and published by . This book was released on 1993 with total page 654 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Zirconium in the Nuclear Industry written by Leo F. P. Van Swam and published by ASTM International. This book was released on 1989 with total page 781 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Handbook of Nuclear Engineering written by Dan Gabriel Cacuci and published by Springer Science & Business Media. This book was released on 2010-09-14 with total page 3701 pages. Available in PDF, EPUB and Kindle. Book excerpt: This is an authoritative compilation of information regarding methods and data used in all phases of nuclear engineering. Addressing nuclear engineers and scientists at all levels, this book provides a condensed reference on nuclear engineering since 1958.
Download or read book Scientific and Technical Aerospace Reports written by and published by . This book was released on 1994 with total page 1028 pages. Available in PDF, EPUB and Kindle. Book excerpt: Lists citations with abstracts for aerospace related reports obtained from world wide sources and announces documents that have recently been entered into the NASA Scientific and Technical Information Database.
Download or read book Zirconium in the Nuclear Industry written by R. B. Adamson and published by ASTM International. This book was released on 1987 with total page 832 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Research on Mechanisms of Stress Corrosion Cracking in Zircaloy written by and published by . This book was released on 1981 with total page pages. Available in PDF, EPUB and Kindle. Book excerpt: The results of internal gas pressurization tests, primarily at 320°C, on cladding tubes from two suppliers, Supplier A and Supplier B, are presented. The two lots show a substantial difference in iodine SCC susceptibility so a test matrix is used to resolve the relative contributions of surface condition, residual stress, and texture. Additional tests with constant deflection split-ring specimens and with unstressed cladding segments are used to understand crack initiation and the early crack growth stages of SCC. The difference in SCC susceptibility is due to crystallographic texture. Other variables such as surface finish, stress relief temperature, and residual stress have little or no effect. Mechanical properties, crack initiation, and crack propagation all depend on texture. Both initiation and propagation features are analyzed by scanning electron microscopy. A mechanism for crack initiation consistent with most observations in this study and with the work of other investigators is proposed. At 320°C, lifetime is crack initiation limited while several tests at 390°C indicate that lifetime is less initiation limited at higher temperature. 31 figures, 9 tables.
Download or read book Nuclear Science Abstracts written by and published by . This book was released on 1975-02 with total page 850 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book ERDA Energy Research Abstracts written by and published by . This book was released on 1983 with total page 1144 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Government reports annual index written by and published by . This book was released on 199? with total page 1216 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Energy Research Abstracts written by and published by . This book was released on 1982 with total page 844 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Physics Briefs written by and published by . This book was released on 1992 with total page 1216 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book CAB Current Awareness Bulletin written by and published by . This book was released on 1979 with total page 478 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Government Reports Announcements Index written by and published by . This book was released on 1984 with total page 1196 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Research in Materials written by Massachusetts Institute of Technology and published by . This book was released on 1981 with total page 488 pages. Available in PDF, EPUB and Kindle. Book excerpt: