Download or read book Effects of Temperature and Frequency on the HCF Behavior of a Ni based Superalloy written by and published by . This book was released on 2005 with total page 11 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Influence of High Frequency Vibrations on the Low Cycle Fatigue Behavior of a Superalloy at Elevated Temperature written by Ouyang J and published by . This book was released on 1988 with total page 11 pages. Available in PDF, EPUB and Kindle. Book excerpt: The influence of relatively high-frequency, low-amplitude vibrations on the low-cycle fatigue (LCF) behavior and its fractographic feature for a GH36 Fe-Ni alloy at 600°C is studied. It is found that the influence is rather complicated and significant. The nature and extent of the influence depended upon the ratio of the amplitude of high-cycle to low-cycle stress range, Q. As Q approaches Qc (the critical value of Q), there is no appreciable influence on the total LCF life; as Q Qc, it will prolong the lifetime slightly; and as Q Qc, the fatigue life will decrease progressively. The variation of fatigue life was ascribed to the occurrence of some considerable interactions between creep, high-cycle fatigue (HCF), LCF, and environmental effect under different values of Q at elevated temperature, and the change of damage mechanism of the material. The total LCF life, especially crack propagation life, will be markedly reduced by the high-cycle vibrations when Q is much greater than Qc. Meanwhile, the mixed failure of creep, HCF, LCF, and environmental attack will gradually change into combined cycle fatigue failure with increasing Q. The fractographic analysis is in agreement with these results.
Download or read book High Temperature Low cycle Fatigue Behaviour of Nickel base Superalloys written by L. Massarelli and published by . This book was released on 1977 with total page 26 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book High Temperature Low cycle Fatigue Behaviour of Nickel base Superalloys Influence of Testing Frequency and Stree Or Strain Wave Form written by L. Massarelli and published by . This book was released on 1977 with total page pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book The Room Temperature Fatigue Behavior of Nickel base Superalloy Crystals at Ultrasonic Frequency written by J. K. TIEN and published by . This book was released on with total page 6 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Superalloys 2020 written by Sammy Tin and published by Springer Nature. This book was released on 2020-08-28 with total page 1098 pages. Available in PDF, EPUB and Kindle. Book excerpt: The 14th International Symposium on Superalloys (Superalloys 2020) highlights technologies for lifecycle improvement of superalloys. In addition to the traditional focus areas of alloy development, processing, mechanical behavior, coatings, and environmental effects, this volume includes contributions from academia, supply chain, and product-user members of the superalloy community that highlight technologies that contribute to improving manufacturability, affordability, life prediction, and performance of superalloys.
Download or read book Low Cycle Fatigue written by Harvey D. Solomon and published by ASTM International. This book was released on 1988 with total page 1289 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Fatigue Behavior of a Nickel Based Directionally Solidified Superalloy at Elevated Temperature written by Louis Domenic Terranova and published by . This book was released on 1989 with total page 232 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book The Effect of Frequency on the Elevated Temperature Fatigue of a Nickel base Superalloy written by F. E. ORGAN and published by . This book was released on with total page 10 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book The Effects of Frequency and Waveshape on the Fatigue Crack Growth of an Advanced Nickel Base Superalloy at Elevated Temperatures written by Sara Dalby and published by . This book was released on 2002 with total page pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book The Effects of Environment on the Elevated Temperature Fatigue Behavior of Nickel Base Superalloy Single Crystals written by D. J. DUQUETTE and published by . This book was released on with total page 7 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book High Cycle Fatigue written by Theodore Nicholas and published by Elsevier. This book was released on 2006-07-07 with total page 657 pages. Available in PDF, EPUB and Kindle. Book excerpt: Dr Theodore Nicholas ran the High Cycle Fatigue Program for the US Air Force between 1995 and 2003 at Wright-Patterson Air Force Base, and is one of the world's leading authorities on the subject, having authored over 250 papers in leading archival journals and books. Bringing his plethora of expertise to this book, Dr Nicholas discusses the subject of high cycle fatigue (HCF) from an engineering viewpoint in response to a series of HCF failures in the USAF and the concurrent realization that HCF failures in general were taking place universally in both civilian and military engines. Topic covered include: - Constant life diagrams - Fatigue limits under combined LCF and HCF - Notch fatigue under HCF conditions - Foreign object damage (FOD) - Brings years of the Author's US Air Force experience in high cycle fatigue together in one text - Discusses HCF in the context of recent international military and civilian engine failures
Download or read book The Superalloys written by Roger C. Reed and published by Cambridge University Press. This book was released on 2008-07-31 with total page 363 pages. Available in PDF, EPUB and Kindle. Book excerpt: Superalloys are unique high-temperature materials used in gas turbine engines, which display excellent resistance to mechanical and chemical degradation. This book introduces the metallurgical principles which have guided their development. Suitable for graduate students and researchers, it includes exercises and additional resources at www.cambridge.org/9780521859042.
Download or read book Nickel Cobalt and Their Alloys written by Joseph R. Davis and published by ASM International. This book was released on 2000-01-01 with total page 450 pages. Available in PDF, EPUB and Kindle. Book excerpt: This book is a comprehensive guide to the compositions, properties, processing, performance, and applications of nickel, cobalt, and their alloys. It includes all of the essential information contained in the ASM Handbook series, as well as new or updated coverage in many areas in the nickel, cobalt, and related industries.
Download or read book International Aerospace Abstracts written by and published by . This book was released on 1999 with total page 974 pages. Available in PDF, EPUB and Kindle. Book excerpt:
Download or read book Multiaxial Fatigue written by Darrell Socie and published by SAE International. This book was released on 1999-12-15 with total page 510 pages. Available in PDF, EPUB and Kindle. Book excerpt: This book provides practicing engineers, researchers, and students with a working knowledge of the fatigue design process and models under multiaxial states of stress and strain. Readers are introduced to the important considerations of multiaxial fatigue that differentiate it from uniaxial fatigue.
Download or read book Gigacycle Fatigue in Mechanical Practice written by Claude Bathias and published by CRC Press. This book was released on 2004-09-13 with total page 327 pages. Available in PDF, EPUB and Kindle. Book excerpt: Written by pioneers in the study and analysis of very high cycle fatigue this text brings together the most recent findings on gigacycle fatigue phenomena, focusing on improving the reliability and performance of key engine and machine components. This reference reflects the explosion of new concepts, testing methods, and data on very high cycle fa